 Test report of the world second biggest OEM factory
 Test report of the world second biggest OEM factory



Initial Sample Test in LF Solder Pot
Solder dross before and after treatment:
 
Heavy solder dross on surface of pot, 99% are solder and tin oxidation
Cement like dross, almost are carbide and organic compounds on surface of pot

Quantitive Dross Remover Evaluation
One LF wave pot and one Pb wave pot in Bu6 and Bu3 respectively were selected to do evaluation on real production line.
Evaluation step:
Remove all solder dross in the wave pot
Add around 350ml dross remover to the pot surface to form a thin layer
In producing, add 100~200 ml every 3~4hours to prevent dross generation(no product, no need to add and just need to monitor and add 50ml to keep the layer on the surface on pot
Record liquid consumption and dross quantity every day until the dross remover used up


Bu6 LF Wave Pot Try Run
Step: Clean up all solder dross in the pot

 Add the first batch of JR07-VI to protect the surface of pot
 Add one stainless breakwater in pot to prevent the chemical dispersing on solder surface
For bu6 LF wave, first amount is around 350ml, after 4 hours, add 110 to keep the working status of this reductant. (Evaluation period: 10-24~11-02 2007)
  
Before add reductant                                       After add reductant

のS4ページ:[1] 2 [3] [4]
 

      Member Center
 
Username:
Password:

Copy Right: Shenzhen Kunqi Xinhua Co., Ltd.
Add: Room 1301-2, Apartment C, Block 3, Tian'an Cloud Park, Bantian Subdistrict, Longgang  District, Shenzhen City, China 518129
Contact us : 18126259136(Yan yao),18923487296(Changchun Yan)
Tel: (86) 0755-89253020; 89253221   Fax: (86) 0755-89253332
E-mail: nobeyan@szkqxh.com